Ni200/201 - UNS N02200 | Pure Nickel

Nickel, Cobalt, and Titanium Alloys

Nickel Alloys

Ni200/201 - UNS N02200 | Pure Nickel

Overview & Features

Pure Nickel has high corrosion resistance to many medium, as well as high electrical and thermal conductivity, and is used in a variety of applications, such as chemical plants, electrical and electronic components, aerospace, and automobiles.
It has excellent ductility and cold workability, but since it is a soft material, care must be taken when cutting it.

Available Shapes

Standards are listed as equivalent or similar to our materials, so please use them as a reference.

UNS

N02200
N02201

JIS

NW2200, H4554
NW2201, H4554

ISO

NW2200, Ni99.0
NW2201, Ni99.0-LC

GB

NW2200, Ni99.0
NW2201, Ni99.0-LC

[Composition] Ni99.0/Ni99.0-LC

Density

8.9 g/cm³

Thermal Expansion

11.9×10-6/K

SEARCH MATERIALS

Search by
Material Properties

Search by
Tensile Strength [MPa]

Search by
Yeild Strength [MPa]

Search by Elongation [%]

Search by Hardness [HV]

Search by Categories

Search by Keyword
(Grades, Features, Standards, etc.)