HC-22 (HASTELLOY® C22 Equiv.) - UNS N06022-ASTM B575

  1. HOME
  2. SEARCH MATERIALS
  3. Nickel, Cobalt, and Titanium Alloys
  4. Nickel Alloys
  5. HC-22 (HASTELLOY® C22 Equiv.) - UNS N06022-ASTM B575

Nickel, Cobalt, and Titanium Alloys

Nickel Alloys

HC-22 (HASTELLOY® C22 Equiv.) - UNS N06022-ASTM B575

Overview & Features

HC-22 has excellent overall corrosion resistance among Ni-Cr-Mo alloys.
It has extremely excellent resistance to reducing and oxidizing corrosive environments, and is used in applications where reduction and oxidation are repeated.
We provide HASTELLOY C22 or its equivalent material.
*HASTELLOY® is a registered trademark of Haynes International, Inc.

Examples of Applications

Bellows, Fuel Gas Desulfurization Equipment

Available Shapes

For inquiries regarding procurement items (Pipes, bars, Wires etc.), please contact us.

Manufacturable Range (COIL, SHEET)

Thickness

0.020-1.00mm  

Width

3.0-300mm

Length

COIL or SHEET less than 2000mm

This is the manufacturing range of coils and sheets we manufacture.

Standards are listed as equivalent or similar to our materials, so please use them as a reference.

UNS
ASTM

N06022
B575

JIS

NW6022 - G4902 (Strip, Sheet)

ISO

NW6022, NiCr21Mo13Fe4W3

Density

8.69 g/cm³

Specific Heat

414 J/(kg・K) (21℃)

Electrical Resistivity

114 μΩ・cm (21℃)

Young's Modulus

206 GPa

Thermal Expansion

12.4×10-6/K(20~100℃)

Thermal Conductivity

11.1 W/(m・K) (21℃)

Mechanical properties in the annealed condition are as follows

TSM catalogue

High Corrosion Resistance Alloys
Heat Resistance Alloys

Please click on the button to proceed to the download.

Superalloys(Nickel, Cobalt, and Titanium Alloys)

Materials based on Ni, Co, and Ti are superior to stainless steel in terms of corrosion resistance and heat resistance. In addition to cold-rolled strips manufactured by our company, we also provide thick plates, wires, bars, and ultra-thin pipes sourced from domestic and overseas partner companies for you.

Metal Foils (Under t0.10mm)

We can produce foil materials in all the materials we manufacture, from stainless steel, low carbon steel, high carbon steel, and other steel materials to nonferrous metals such as nickel alloys, cobalt alloys, and copper alloys.

Materials for Bellows

We manufacture TOKKIN 350 and various other metals for bellows, and we can propose materials and specifications according to required properties such as strength, corrosion resistance, and heat resistance.

SEARCH MATERIALS

Search by
Material Properties

Search by
Tensile Strength [MPa]

Search by
Yeild Strength [MPa]

Search by Elongation [%]

Search by Hardness [HV]

Search by Categories

Search by Keyword
(Grades, Features, Standards, etc.)