Nickel, Cobalt, and Titanium Alloys
Nickel Alloys

Standards are listed as equivalent or similar to our materials, so please use them as a reference.
UNS
ASTM
N10675
B333

Density
9.22 g/cm³
Electrical Resistivity
137 μΩ・cm
Materials based on Ni, Co, and Ti are superior to stainless steel in terms of corrosion resistance and heat resistance. In addition to cold-rolled strips manufactured by our company, we also provide thick plates, wires, bars, and ultra-thin pipes sourced from domestic and overseas partner companies for you.
We can produce foil materials in all the materials we manufacture, from stainless steel, low carbon steel, high carbon steel, and other steel materials to nonferrous metals such as nickel alloys, cobalt alloys, and copper alloys.