Alloy 90

Overview & Features

Alloy 90 is a precipitation hardening alloy with excellent corrosion and oxidation resistance, and with high creep resistance at temperatures up to 920°C.

Available Shapes

Standards are listed as equivalent or similar to our materials, so please use them as a reference.

UNS

N07090

AMS

5829

Density

8.18 g/cm³

Superalloys(Nickel, Cobalt, and Titanium Alloys)

Materials based on Ni, Co, and Ti are superior to stainless steel in terms of corrosion resistance and heat resistance. In addition to cold-rolled strips manufactured by our company, we also provide thick plates, wires, bars, and ultra-thin pipes sourced from domestic and overseas partner companies for you.

Metal Foils (Under t0.10mm)

We can produce foil materials in all the materials we manufacture, from stainless steel, low carbon steel, high carbon steel, and other steel materials to nonferrous metals such as nickel alloys, cobalt alloys, and copper alloys.

SEARCH MATERIALS

Search by
Material Properties

Search by
Tensile Strength [MPa]

Search by
Yeild Strength [MPa]

Search by Elongation [%]

Search by Hardness [HV]

Search by Categories

Search by Keyword
(Grades, Features, Standards, etc.)