Beta 21S

Overview & Features

Beta 21S is metastable beta titanium that can be cold worked and has high oxidation resistance properties.

Available Shapes

Standards are listed as equivalent or similar to our materials, so please use them as a reference.

UNS

R58210

ASTM

B265

Density

4.93 g/cm³

Electrical Resistivity

1.35 μΩ・cm

Superalloys(Nickel, Cobalt, and Titanium Alloys)

Materials based on Ni, Co, and Ti are superior to stainless steel in terms of corrosion resistance and heat resistance. In addition to cold-rolled strips manufactured by our company, we also provide thick plates, wires, bars, and ultra-thin pipes sourced from domestic and overseas partner companies for you.

Metal Foils (Under t0.10mm)

We can produce foil materials in all the materials we manufacture, from stainless steel, low carbon steel, high carbon steel, and other steel materials to nonferrous metals such as nickel alloys, cobalt alloys, and copper alloys.

SEARCH MATERIALS

Search by
Material Properties

Search by
Tensile Strength [MPa]

Search by
Yeild Strength [MPa]

Search by Elongation [%]

Search by Hardness [HV]

Search by Categories

Search by Keyword
(Grades, Features, Standards, etc.)